| KARAKTERISTIKAT TEKNIKE | METODA E TESTIMIT | STANDARD | NEX-GEN |
| MATJA DHE PARAQITJA E SIPËRFAQËSISË | |||
| GJATESIA DHE GJERESIA | EN ISO 10545-2 | ±0,6% | -0,26% ~-0,14% |
| ±2 mm | -0.5mm ~+0.6mm | ||
| TRASHËSIA | EN ISO 10545-2 | ±5% | -0.4% ~+0.9% |
| ±0,5 mm | -0.6mm ~+0.5mm | ||
| DREJTËSIA E ANËVE | EN ISO 10545-2 | ±0,5% | +0,01% ~+0,03% |
| ±1,5 mm | +0,08mm ~+0,19mm | ||
| VETITË FIZIKE | |||
| THYRTIMI I UJIT | EN ISO 10545-3 | E> 10% | 15,70% |
| THYERJA E FORCËS | EN ISO 10545-4 | ≥600N | 1368 |
| MODULI I RUPTURËS | EN ISO 10545-4 | ≥12N/mm² | 24.9 |
| REZISTENCA NDAJ gërryerjes | EN lSO 10545-7 | RAPORTI NË KLASËN E ABRAZIONIT | KLASA 3 |
| CIKLET E RAPORTIT TË KALUARA | 1, 500 r | ||
| REZISTENCA E CRAZHUR | EN ISO 10545-11 | REZISTENCË E PLOTË | KALOJE |
| REZISTENCA NGA NGRITJA | EN ISO 10545-12 | REZISTENCË E PLOTË | KALOJE |
| VETITË KIMIKE | |||
| REZISTENCA KIMIKE TE KIMIKAT E FAMILJEVE & KRIPËRA TË PISHINAVE | EN ISO 10545-13 | MINIMUM GB | A |
| REZISTENCA NDAJ NJOLJES | EN lSO 10545-14 KUR I SUBJEHET KIMIKAVE | KLASA MINIMUM 3 | Klasa 5 |
| SERIA | PËRMASAT | PCS/CTN | M²/ CTN | M²/PLT | CTN / PLT | KG/PLT |
| ZBEHET | 200x600mm/8"x24" | 10 | 1.2 | 26.4 | 64 | 1408 |
*Pllakat mund të ndryshojnë në madhësi, peshë, ngjyrë, model, lyerje, strukturë, qëndrueshmëri, dendësi, sipërfaqe dhe përfundim nga grupi në grup.Vlerësimet e rrëshqitjeve shërbejnë si tregues dhe mund të ndryshojnë për çdo grup pllakash.Rekomandohet që të kryhet një test i ri për çdo grup pllakash nëse kërkohet një certifikatë e vlerësimit të rrëshqitjes.Imazhet e treguara të produktit janë vetëm për qëllime ilustrimi dhe nuk janë një paraqitje e saktë e produktit.