| CARATTERISTICHE TECNICHE | METODU DI TEST | STANDARD | NEX-GEN |
| MISURA E APPARENZA DI SUPERFICIE | |||
| LUNGHEZZA E LARGHE | EN ISO 10545-2 | ± 0,6% | -0,01% ~ + 0,01% |
| ± 2 mm | -0,05 mm ~ + 0,2 mm | ||
| SPESSORE | EN ISO 10545-2 | ± 5% | -0,11% ~ + 1,26% |
| ± 0,5 mm | -0,1 mm ~ + 0,1 mm | ||
| DRITTEZZA DI LATI | EN ISO 10545-2 | ± 0,5% | -0,04% ~ -0,02% |
| ± 1,5 mm | -0,3 mm | ||
| PROPRIETATI FISICHE | |||
| ASSORBTION D'ACQUA | EN ISO 10545-3 | ≤0,5% | ≤0,1% |
| FORZA DI RUPTURA | EN ISO 10545-4 | ≥1300N | 1984 |
| MODULU DI RUPTURA | EN ISO 10545-4 | ≥35 N/mm² | 36 |
| RESISTENZA À L'ABRASION | EN ISO 10545-7 | RAPPORTU À A CLASSE ABRASION | Classe 4 |
| RAPPORTU CYCLES PASSATU | 2.100 r | ||
| RESISTENZA A SHOCK THERMAL | EN ISO 10545-9 | NESSUN DIFETTU DEVA ESSERE VISIBILE | PASSU |
| RESISTENZA FROST | EN ISO 10545-12 | NO DIFETTI DI SUPERFICIE OR I CRACKS DEVERU ESSERE VISIBILI | PASSU |
| SLIDER 96 RESISTENZA GLI SCIVOLI, TEST PENDULUM UMIDI | SECONDO AS 4586:2013 | - | |
| MATT | P3 | ||
| ESTERNI | P4 | ||
| PROPRIETÀ CHIMICA | |||
| RESISTENZA CHIMICA A CHIMICA DOMESTIA & SALI PISCINA | EN ISO 10545-13 | MINIMUM GB | A |
| RESISTENZA À STAINING | EN ISO 10545-14 | CLASSE MINIMA 3 | CLASSE 5 |
| SERIE | TAGLIE | PCS/CTN | M²/ CTN | M²/PLT | CTN/PLT | KG/PLT |
| QUERCIA | 200x1200mm/8"x48" | 4 | 0,96 | 43.2 | 45 | 1057,5 |
* U tile pò varià in dimensioni, pesu, culore, mudellu, venature, texture, durabilità, densità, superficia è finitura da lotto à lotto.A classificazione di slip serve com'è indicazione è pò varià per ogni batch of tile.Hè ricumandemu chì una nova prova sia realizata per ogni batch di piastrelle se un certificatu di valutazione di slip hè necessariu.L'imaghjini di u produttu mostrati sò solu per scopi illustrativi è ùn sò micca una rappresentazione esatta di u pruduttu.